A182
SS400一般構造用壓延鋼材
化學成份:JIS G3101
| 牌號 | 碳C | 錳Mn | 磷P | 硫S |
| SS300 | -- | -- | ≦0.05 | ≦0.05 |
| SS400 | -- | -- | ≦0.05 | ≦0.05 |
| SS490 | -- | -- | ≦0.05 | ≦0.05 |
| SS540 | ≦0.3 | ≧1.6 | ≦0.04 | ≦0.04 |
機械性質:JIS G3101
| 牌號 | 降伏強度Mpa | 抗拉強度Mpa | |||
| 厚度mm | |||||
| <16 | 16-40 | 40-100 | >100 | ||
| SS300 | ≧205 | ≧195 | ≧175 | ≦0.05 | 330-430 |
| SS400 | ≧245 | ≧235 | ≧215 | ≦0.05 | 400-500 |
| SS490 | ≧285 | ≥275 | ≧255 | ≦0.05 | 490-610 |
| SS540 | ≧400 | ≥390 | -- | -- | ≧540 |